Hot News
- 2025 The 22nd QTG Polyurea Technology Training Course (Qtech Training Group, QTG) Enrollment Notice
- Congratulations on the success of the 21st QTG polyurea technology training course
- 2024 The 21st QTG Polyurea Technology Training Course (Qtech Training Group, QTG)
- Academician Sergei Leonovich was invited to visit Qingdao Shamu Advanced Material Co., Ltd.
- In Memoriam of Ding Defu
- Congratulation 60 Years Old of Dudley J. Primeaux
- Pure polyurea is not afraid of testing , just like real gold is not afraid of fire
- The preparation of the second edition of spray polyurea elastomer technology has come to an end
Experts
Prof. Weibo HuangGraduated from Sichuan University in 1986 andjoined MCRI (Marine Chemical Research Institute) the same year.
Mr. Dudley J. PrimeauxReceived an M.S. Degree in Organic Chemistry from Lamar University in Beaumont, Texas in 1984.
Raw material
- Qtech-114 Aliphatic Polyurethane Top Coat
- Qtech-112 All Weather Surface Preparation System
- Qtech-404 Mining Equipment Ultra Anti-Abrasion Polyurea Material
- Qtech-400 High Speed Railway Sub Grade Polyurea Protective Coating
- Qtech-406 Elastomer Waterproofing Material
- Qtech-407 Anti-Microbial Polyurea Material
- Qtech-411 Bridge Ultra-Long Service Life Polyurea Material
Equipments
Surface preparation
Surface must be properly prepared. Remove
all oil, dust, grease, dirt, loose, and foreign
materials to ensure adequate adhension.
Steel: Surfaces must be a "near white
metal" blast to SIS-Sa 2 1/2. With a
3 mil profile. Prime with anticorrosive primer
prior to spraying. Steel surfaces shall be
dry and clean, free from any dirt, grease,
oil and other contamination before priming
and spraying.
Concrete: Concrete
surfaces prepared according to NACE standard
RP0892-92. Allow substrate to dry thoroughly
prior to priming (minimum substrate of new
concrete cure is 28 day). Remove all from
loose dust or other foreign matter and prime
with primer sealing primer at 1~2 coats prior
to spraying.
Fiber Reinforced Plastic (FRP):Remove
all foreign material from surface and prime
with anticorrosive primer at at 1~2 coats
prior to spraying.
EVA/Polyurethane foam (PUF): Directly spray without any surface preparation.